A high-quality Cr3+:CdWO4 single crystal at a size of approximately \Phi 25 \times 80 mm is grown using the Bridgman method with CdO, WO3, and Cr2O3 as raw materials and their molar ratio of 100:100:0.5. The temperature gradient of solid-liquid interface at growth is approximately 50 oC/cm and the g